File:Ta C wear (original).jpg
Size of this preview: 275 × 598 pixels. Other resolutions: 110 × 240 pixels | 221 × 480 pixels | 672 × 1,461 pixels.
Original file (672 × 1,461 pixels, file size: 190 KB, MIME type: image/jpeg)
Summary
Scanning Tunneling Microscopic (STM) image of surfaces at the edge of a 1 μm thick layer of ta-C "diamond-like" coating on 304 stainless steel after various durations of tumbling in a slurry of 240 mesh SiC abrasive. The first 100 min shows a burnishing away from the coating of an overburden of soft carbons than had been deposited after the last cycle of impacts converting bonds to sp3. On the uncoated part of the sample about 5 μm of steel were removed during subsequent tumbling while the coating completely protected the part of the sample it covered.
Licensing
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 19:06, 27 October 2006 | 672 × 1,461 (190 KB) | Drac2000 (talk | contribs) | ||
| 22:25, 25 October 2006 | 402 × 290 (31 KB) | Drac2000 (talk | contribs) |